Pipe. Connect. Future.
Home
Products
ServicesCalculatorAbout us Contact Request a quote

1.4541

1.4541 (321) is a titanium-stabilised austenitic stainless steel – intergranular-resistant even at higher temperatures, without molybdenum.

Austenitic stainless steelNo. 1.4541X6CrNiTi18-10
1.4541
Material no.
≥ 200 MPa
Yield strength Rp0.2
500–720 MPa
Tensile strength Rm
intergranular-resistant to ~400 °C · scaling-resistant to ~800 °C
Service temp.
Application

Application & properties

1.4541 (321) is a titanium-stabilised austenitic stainless steel – intergranular-resistant even at higher temperatures, without molybdenum.

  • Exhaust and heat-exchanger construction
  • Chemical and process plants at higher temperatures
  • Welded apparatus and piping
Chemistry

Chemical composition

Typical values in wt.-% per EN standard (heat analysis).

ElementContent (%)
C≤ 0.08
Si≤ 1.00
Mn≤ 2.00
Cr17.0–19.0
Ni9.0–12.0
Ti5×C–0.70
Mechanics

Mechanical properties

Typical values at room temperature per EN standard.

PropertyValue
Yield strength Rp0.2≥ 200 MPa
Tensile strength Rm500–720 MPa
Elongation A≥ 40 %
Standards & supply

Standards, equivalents & product forms

TopicDetail
StandardsEN 10216-5, EN 10088
ASME/ASTM equivalent~ AISI 321
Material no.1.4541
Short name / akaX6CrNiTi18-10 · AISI 321

We supply 1.4541 as pipes, flanges and fittings – seamless or welded, on request with an EN 10204 3.1 / 3.2 mill certificate.

FAQ

Frequently asked questions about 1.4541

What is the difference between 1.4541 and 1.4571?

Both are titanium-stabilised; 1.4571 (316Ti) additionally contains molybdenum and is thus more chloride-resistant, while 1.4541 (321) is molybdenum-free.

What is 1.4541 typically used for?

For higher-temperature welded applications such as exhaust lines and heat exchangers.

Request 1.4541?

Grade, standard, size, pressure rating and quantity are enough – on request with an EN 10204 3.1 / 3.2 mill certificate. Your quote usually the same day.

All data are typical values per the relevant EN standards for first orientation – without warranty. The applicable standard and the mill certificate of the delivery are decisive.